Abstract
Gallium nitride (GaN) is one of the most important semiconductor materials in modern electronics. While GaN films are routinely deposited by chemical vapor deposition at around 1000 °C, low-temperature routes for GaN deposition need to be better understood. Herein, we present an atomic layer deposition (ALD) process for GaN-based on triethyl gallium (TEG) and ammonia plasma and show that the process can be improved by adding a reactive pulse, a “B-pulse” between the TEG and ammonia plasma, making it an ABC-type pulsed process. We show that the material quality of the deposited GaN is not affected by the B-pulse, but that the film growth per ALD cycle increases when a B-pulse is added. We suggest that this can be explained by the removal of ethyl ligands from the surface by the B-pulse, enabling a more efficient nitridation by the ammonia plasma. We show that the B-pulsing can be used to enable GaN deposition with a thermal ammonia pulse, albeit of x-ray amorphous films.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.