Abstract

Peri-implantitis is one of the most common complications after dental implant placement. Researchers have demonstrated that the peri-implantitis tends to occur around dental implants with a rough surface rather than those with a smooth surface. We aimed to investigate the ability of a smooth titanium (Ti) surface containing strontium (Sr) to enhance bone formation as a result of strontium's capacity to support osteoblast proliferation and differentiation. A thin titanium oxide film was formed on an as-mirror polished Ti surface by dipping in 5% sodium hypochlorite (NaOCl) solution for 24 h, followed by thermal treatment at 350°C. The Ti surface was then treated with 1% strontium nitrate (Sr(NO3)2) solution and turned in spin coater. The surface morphology, chemical composition, and release of strontium ions (Sr2+) were evaluated. The results demonstrate that strontium in the form of Sr2+ was successfully doped into the titanium dioxide (TiO2) film by this simple chemical treatment.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.