Abstract
Surface Analysis III: The recent demonstration of the tunneldiode effect on an atomic scale forms the basis of this article which also looks at the overall trends towards miniaturazation of devices down to the atomic scale. The latest achievement is based on the ability of the scanning tunneling microscope (STM) to image regions of negative differential conductivity on the surface of boron doped silicon.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.