Abstract

Three point bend set up is used to evaluate load and load point displacement on specimen during dynamic condition. Here, experiments have been conducted on Al 6063 alloys on Modified Hopkinson Pressure Bar (MHPB) in dynamic condition. The cylinder pressure and striker velocity was measured during experiments and it was 3.1 bar and 24m/s respectively. The strain gauges, data acquisition computer were used to measure strain at two points at Hopkinson bar. The load point displacement and load are obtained by the two point strain measurement methods and one dimensional wave theory in terms of strains measured experimentally at two points.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.