Using the hydrolysis reaction of TEOS and ethanol to prepare nano-SiO2 sol, and grafting with silane coupling agent WD-20 to introduce double bonds to make a surface modification, the nano-SiO2 sol mixed with the light-cured resin PEA, reactive diluents TPGDA and photoinitiators 1171 under ultrasonicto after dried concentration in vacuum oven, then the composite resin gotten was characterized through FTIR, TGA, UV-Vis and particle size analysis. The results showed as follows: the light-cured resin modified by nano-SiO2 with WD-20 was better in dispersion and stability, and durability, abrasion resistance and other performances of the coating improved significantly which broadened the application range of light-cured resin.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.