Abstract

This research through the study on the properties of silicon dust, put forward in combination with lime kiln tail gas recycling carbon dioxide, preparation of precipitated silica (nanoWhite Carbon Black) of high value utilization technology, and studied and summarized process of the dissolution and precipitation by carbon dioxide. The silica fume is in amorphous form, and it has some special powder properties such as ultra fine grain size and high specific surface area and high chemical activity, these provide favorable foundation for low energy consumption process of recycling the powder. In the dissolution stage, the optimization reaction time is about 40 minutes, this time to complete the process of the reaction more than 90%. And the reaction is the fastest in the first 20 minutes, complete response 75% of the reaction. In the stage of carbonization, with increase of the concentration of the precursor, the particle diameter becomes larger, but the specific surface area of the powder will reduce, the porosity and the surface activity of it will reduce corresponding.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call