Abstract
Two AISI (316,304) stainless steel alloys were utilized in this work to enhance the surface properties and corrosion inhibiters with Al2O3 nanoparticles which was generated via pulse laser deposition (PLD). Alumina as biomaterial for dental purposes was prepared using the co-precipitation process and analysis by X-Ray diffraction. Alumina has drawn a lot of interest and is historically well-accepted .SEMs, and EDS, been used to describe researchers have studied the coating morphology. Roughness and Vickers hardness were utilized to quantify the surface modifications as part of an investigation into corrosion prevention employing mechanical properties submerged in saliva with a PH (5.6). When compared to bare AISI (316,304) stainless steel, all samples exhibit greater corrosion resistance.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.