Abstract

An inert ceramic ball was prepared by using three kind of raw materials i.e. Selendang clay, silica sand, feldspar and distilled water. Selendang clay, silica sand, feldspar and distilled water were pre-mixed manually and compounded using a beaker. Universal testing machine (UTM) was used to test mechanical strength. Electron scanning microscope (SEM-EDX) was used for the study morphological feature and element mapping in the ceramic balls. X-ray powder diffraction (XRD) was used to determine the phase of crystalline material. The optimum sintering temperature was 1300 °C23 and got the strength of 238.8 kgf.