Abstract
Recent studies on stress corrosion cracking properties of 321 bend pipe and pipe with weld, 316NG austenitic stainless steel pipe in ocean environment in virtue of slow strain rate tensile stress corrosion crack test are performed in different concentration of NaCl solution. Elongation and max tensile stress are selected as parameters to evaluate the SCC susceptibility based on the phenomenon that elongation and max stress fall as samples being exposed to NaCl solution environment, the results show that 316NG has the best stress corrosion crack resistance and 321 bend pipe materials behavior oppositely. In addition, the influence of differing strain rate and concentration of NaCl solution on properties of materials are researched, elongation increases along with tensile strain rate enhancement, mechanical properties are immune to variety of Cl- concentration from 3.5% to 26.5%.