Abstract
Aiming at the problem that sapphire surface roughness is quite large after wet etching in sapphire microstructure processing technology, we optimize the wet etching process parameters, study on the influences of concentration and temperature of etching solution and etching time on the sapphire surface roughness and etching rate, choose different process parameters for the experiment and test and analyze the sapphire results after wet etching. Aiming at test results, we also optimize the process parameters and do experiment. Experimental results show that, after optimizing the parameters of etching solution, surface roughness of etched sapphire is 0.39 nm, effectively with reduced surface roughness, improved light extraction efficiency and meeting the production requirements of high-precision optical pressure sensor.