Abstract
The paper deals with the physical properties of colloidal silica dispersed system such as distribution width (Qx, %) and density (qx, %) defined by photon cross correlation spectroscopy (PCCS) at an average size of 17.06 nm for D50 % and the area of specific surface of 349.96 m2 cm−3 depending on molar (Rm2) optimal ratio of silica stone mineral to alkali ash powder. The change of crystal structure to amorphous state was determined by X-ray diffraction analysis. The results of their kinematic viscosity, liquid density, UV light adsorption inspections show possibility to produce the colloidal silica by using the wetting and ultrasonic vibration method for that fusible alloy.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.