InN films were grown by RF-MBE on (0001) sapphire substrates. Nitridation of the sapphire substrate prior to growth was carried out at 280degC for 2 hours. After a low-temperature InN buffer layer was deposited at 280degC for 10 min, InN intermediate layer was grown at 530degC for 10 min. Then, non-and Mg-doped InN layers were grown at 530degC for 1 hour under a nitrogen-rich condition. Mg was supplied by a conventional effusion cell at 130, 135, or 140degC. The thicknesses of the InN films were around 420 nm. All InN films were characterized using XRD, SEM, and Hall-effect measurements.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.