Aluminum borate whisker with different ratios (20wt%, 30wt%, 40wt%, 50wt%, 70wt%) was added to the aluminum phosphate matrix. The composite was sintered at 750 ℃ -1400 ℃ temperature, then the dielectric constant ( e ) and the dielectric loss tangent (tan δ ) of the composite was measured. The results show that when the whisker content is the same, the dielectric constant of the sample increases with increasing of relative density, but the dielectric loss decreases with increasing of relative density. The dielectric loss of the composite is mainly caused by the relaxation polarization.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.