Abstract

A chrome gel system with 13 million molecular weight and 19 million molecular weight polymer and DQ-8 cross-linking agent is dynamically gelled under different conditions of 50-mesh and 100-mesh screens under different shear rates. Concentration limit. The experiment shows that the critical concentration of 13 million molecular weight gelation is 500-700mg/L, and the critical concentration of new cross-linking agent in the system is 80mg/L-90mg/L. The system of new cross-linker is cut by steel mesh. The post-gelation time is prolonged. Between 6h-10h, after 12 days of testing, the viscosity of the chrome gel system after gelation can still remain above 1000mPa·s, and the viscosity of the ungelatinized solution drops below 10mPa·s.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.