Abstract

The paper presents the results of wear tests for the SMIC of the titanium - iron system, obtained by the technology, including explosion welding and subsequent high-temperature heat treatment, when the abrasive is exposed to the metal-intermetallic layers at an angle of 0, 45 and 90º. It is shown that more uniform wear is observed when an abrasive is applied to the layered structure of SMIC at an angle of 45º. With such a wear pattern, the best indicators of wear resistance are provided, exceeding the corresponding values for 08kp steel and VT1-0 titanium, and having a tendency to increase with increasing test temperature: +7% at 200 °C; + 13% at 400 °C and + 17% at 600 °C.