Abstract

The paper presents comparative studies of the thermomechanical properties of ultra-high molecular weight polyethylene (UHMWPE) and its composite containing 0.5% coke-graphite powder (CGP). It was found that explosive pressing with a pressure of 0.25-0.6 GPa provides high heat resistance of UHMWPE and the investigated composite (154-156 ° C). The heat resistance of the composite decreases to 143-145 ° C, but it is higher than that of a similar material after static pressing (128 ° C).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.