Abstract
It is shown that the formation of a coating from FeAl/Fe3Al/Fe(Al) iron aluminides on the steel surface of the hopper of the anode mass mixer reduces its sticking to the walls of the funnel during loading. The latter is due to the maintenance of a high temperature of the anode mass due to the low thermal conductivity of the coating in contact with it.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.