Abstract

AbstractThis research investigated the effect of using micro‐nano bubbles and superplasticizers on the rheology of self‐compacting concrete (SCC). Eight mix designs were made with different values of 4–5.5 kg/m3 of superplasticizer. For comparison, half of the mix designs were made with micro‐nano bubbles, and the rest were made with tap water. Flowability, passing ability, and rheological tests were performed on all mixed designs. The results show that an increased rate of superplasticizer from 4 to 5 kg/m3 improved flowability and passing ability in all specimens. The yield stress and plastic viscosity of SCC reduction were higher in samples made with micro‐nano bubbles. The shear‐thickening behavior was observed in SCC samples produced with tap water and the superplasticizer, and the c/μ (positive) ratio increased. While in SCC with micro‐nano bubbles, the shear‐thinning behavior was observed, and the c/μ (negative) ratio increased with increasing the superplasticizer dose.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.