Abstract

We report studies on the magnetocaloric effect of samarium doped lanthanum manganites with different Sm-concentrations. Polycrystalline La0.7-xSmxCa0.30MnO3 (0≤x≤0.3) samples were prepared using the conventional solid-state reaction method with phase purity and structure confirmed using X-ray diffraction. Temperature dependent magnetization measurements and Arrott analysis reveal first order ferromagnetic transition in parent sample and second order ferromagnetic transition in doped sample with Curie temperature decreasing progressively with increasing Sm concentration from ∼182 K for x = 0.05 to 109 K for x = 0.30. A large magnetic entropy change (∼1.75 J kg-1 K-1 at 0.5 T) has been observed in La0.7Ca0.3MnO3 sample, and is greatly suppressed as a function of disorder caused by Sm doping. This is ascribed to the gradual loss of first-order ferromagnetic transition. This investigation suggests that La0.7-xSmxCa0.30MnO3 compounds can be used as a potential magnetic refrigerating material with wide range of temperature.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.