Abstract

Barium titanate nanofibers were uniaxially aligned by electrospinning onto a rotating copper wire drum and alignment was maintained during calcination of the fibers. Two methods for maintaining alignment during calcination were tested, by either using carbon tape or a peeling off method to remove the aligned fibers from the mandrel followed by calcination. The carbon tape removal method led to the formation of shorter aligned nanowires while the peeling off method resulted in longer nanofibers. Additionally, the effects of calcination temperature and time on crystal structure were also examined. The degree of tetragonality in the barium titanate nanofibers increased at higher calcination temperatures and times. Piezoelectricity was confirmed in the nanofibers calcined using piezoeresponse force microscopy, yielding a d33 value of 15.5 pm/V. Using the methods presented here, large quantities of aligned piezoelectric barium titanate and other ceramic fibers or wires can be produced to fulfill their demand in novel microelectronics.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.