Abstract
Crystalline Zn(1−x) Si(x) O(0 ≤ x ≤ 0.156) nanoparticles reveal decreasing particle size with increasing Si content and a undistorted wurtzite form until x = 0.062 beyond which local deformation is observed maintaining the parent structure. There is a sharp increment in bandgap with nominal Si-doping and then almost saturates onwards. Moreover thermal annealing demonstrate the increase bandgap and decreasing lattice parameters. The details of samples synthesis and characterization is presented in the present manuscript.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.