Abstract

The structural characteristics of zinc oxide (ZnO) films deposited on the (0001)- or (11−20)-oriented sapphire substrates were investigated. ZnO films having low temperature ZnO buffer layers were prepared by atomic layer deposition using diethylzinc and nitrous oxide. The ZnO films were analyzed using cross-sectional transmission electron microscopy, high-resolution transmission electron microscopy and x-ray diffractometry. Cross-sectional high-resolution transmission electron microscopic observations showed the presence of extrinsic stacking faults along with Frankel partial dislocations in ZnO near the ZnO/sapphire heterointerface. Based on the results of cross-sectional transmission electron microscopic observations and double-crystal x-ray rocking curve measurements, it was found that buffer-layer annealing treatment tended to reduce the density of threading dislocations in a ZnO film efficiently so that the crystalline quality of the film was greatly improved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call