Abstract
In this work, corrosion at the tip of stress corrosion cracks on an X65 pipeline steel was investigated under various stress levels in a near-neutral pH solution. Electrochemical and micro-electroc...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.