Abstract The resistance of commercial austenitic, ferritic, and duplex alloys to stress corrosion cracking in a 5% NaOH-2% Na2S-2% Na2CO3-0.2% Na2SO4-0.1 % NaCl solution at 150° has been studied by...

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.