Abstract
We prepared two kinds of cracks (surface cracks and transfixion cracks) to in situ study stress corrosion cracking of seven-layered (which is denoted as 7 M or 14 M) off-stoichiometric Ni 2MnGa magnetic shape memory alloy in deionized water and moist atmosphere under constant deflection at room temperature. The experimental results showed that the cracks could nucleate and propagate continuously or discontinuously for a distance after some incubation time, and then arrest in water or moist atmosphere under constant deflection. The delayed cracking of Ni 2MnGa alloy is regarded as reduction of the surface energy induced by adsorption of water molecule.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.