Abstract
In general, one may suggest that all the Fe-Co-B-Fe metallic glasses have good corrosion resistance, especially those with high Co content. Additions of Ni, Mn and Mo are known to further enhance the corrosion resistance of metals. In this investigation, the susceptibility of Fe[sub 78]B[sub 13]Si[sub 9], Fe[sub 66]Co[sub 18]B[sub 15]Si[sub 1], Co[sub 66]Fe[sub 4]Ni[sub 1]B[sub 14]Si[sub 15], Co[sub 76]Fe[sub 2]Mn[sub 4]B[sub 12]Si[sub 6] and Co[sub 69] Fe[sub 4]Ni[sub 1]Mo[sub 2]B[sub 12]Si[sub 12] glasses to stress-corrosion cracking in the HCl solution were examined. The examinations were carried out under bending stress.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.