Abstract

Zr has been used for many plants dealing with nitric acid due to its high corrosion resistance. However, stress corrosion cracking (SCC) occurrence has recently been reported on Zr immersed in hot nitric acid. Here corrosion performance and countermeasures against SCC of Zr, Zr-Ti and Zr-Ti-Ta alloys in HNO 3 were studied. Ti has good general corrosion and SCC resistance in highly oxidizing HNO 3, although it is severely attacked in pure HNO 3 at elevated temperatures. Ta is an excellent corrosion resistant material over all concentrations of nitric acid. Alloying Ti and/or Ta into Zr has synergistic effects on improving both the general corrosion and SCC resistance. The optimization of corrosion resistance has been studied in Zr alloys.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.