Abstract
The paper presents a root cause analysis of a steam turbine rotor blade groove cracking. The scope of analyses included material testing and mechanical integrity calculations. In scope of material testing, fracture microstructure was assessed and basic mechanical property characteristics of the rotor discs were determined. In scope of integrity analyses, the stress fields in the blade grooves were calculated and the possibility of cracking due to different mechanisms was assessed. Both calculations and material tests confirmed the stress corrosion cracking to be the root cause of the rotor failure. This was a basis for proposing the rotor discs repair by overlay welding with a lower strength material and modifications to the groove geometry.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.