This paper presents an experimental investigation carried out to study the effects of Ground Granulated Blast Furnace Slag (GGBFS) on strength development of mortar and the optimum use of slag in mortar. Cement was partially replaced with seven percentages (10%, 20%, 30%, 40%, 50%, 60% and 70%) of slag by weight. Ordinary Portland cement (OPC) mortar was also prepared as reference mortar. A total of 400 cube and briquet mortar specimens were cast and compressive as well as tensile strength of the mortar specimens were determined at curing age of 3, 7, 14, 28, 60, 90 and 180 days. Test results show that strength increases with the increase of slag up to an optimum value, beyond which, strength values start decreasing with further addition of slag. Among the seven slag mortars, the optimum amount of cement replacement is about 40%, which provides 19% higher compressive strength and 25% higher tensile strength as compared to OPC mortar. KEY WORDS: Slag; Cement; Mortar; Compressive Strength; Tensile Strength; Hydration. DOI: http://dx.doi.org/10.3329/mist.v3i0.8053

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.