Abstract

ABSTRACTStrain relaxation in passivated Al-0.5% Cu lines was measured using X-ray diffraction coupled with in-situ observation of the formation and growth of stress induced voids. Samples of 1 μm thick Al-0.5% Cu lines passivated with Si3N4 were heated to 380ºC, then cooled and held at 150ºC. During the test, principal strains along the length, width, and height of the line were determined using a grazing incidence x-ray geometry. From these measurements the hydrostatic strain in the metal was calculated and strain relaxation was observed. The thermal cycle was duplicated in a high voltage scanning transmission electron microscope equipped with a backscattered electron detector. The 1.25 μm wide lines were seen to have initial stress voids. Upon heating these voids reduced in size until no longer observable. Once the samples were cooled to 150ºC, voids reappeared and grew. The measured strain relaxation is discussed in terms of void and θ-phase (Al2Cu) formation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.