Abstract

The potential for creating hierarchical domain structures, or mixtures of energetically degenerate phases with distinct patterns that can be modified continually, in ferroelectric thin films offers a pathway to control their mesoscale structure beyond lattice-mismatch strain with a substrate. Here, it is demonstrated that varying the strontium content provides deterministic strain-driven control of hierarchical domain structures in Pb1- x Srx TiO3 solid-solution thin films wherein two types, c/a and a1 /a2 , of nanodomains can coexist. Combining phase-field simulations, epitaxial thin-film growth, detailed structural, domain, and physical-property characterization, it is observed that the system undergoes a gradual transformation (with increasing strontium content) from droplet-like a1 /a2 domains in a c/a domain matrix, to a connected-labyrinth geometry of c/a domains, to a disconnected labyrinth structure of the same, and, finally, to droplet-like c/a domains in an a1 /a2 domain matrix. A relationship between the different mixed-phase modulation patterns and its topological nature is established. Annealing the connected-labyrinth structure leads to domain coarsening forming distinctive regions of parallel c/a and a1 /a2 domain stripes, offering additional design flexibility. Finally, it is found that the connected-labyrinth domain patterns exhibit the highest dielectric permittivity.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call