Abstract

Cultural heritage objects made of wood can be preserved under waterlogged conditions for many years, where decay is slowed down and the wood structure is more or less completely filled with water. Depending on the degree of degradation, finds may collapse and shrink when they are allowed to dry in an uncontrolled manner after excavation, leading to total loss of the object and its information. Conservation measures are taken to prevent damage of objects and dimensional stability is an important criterion. In this study, structured-light 3D scanning and micro-computed tomography were used to analyse the dimensional stability of wood after conservation, as well as its long-term stability. 83 samples from a reference collection established between 2008 and 2011 allowed this comparative study of the most common conservation methods at that time. The effects of conservation methods using alcohol-ether resin, melamine-formaldehyde (Kauramin 800®), lactitol/trehalose, saccharose, and silicone oil on dimensional stability were investigated. In addition, different polyethylene glycol (PEG) treatments with subsequent freeze-drying were also investigated: one-stage with PEG 2000, two-stage with PEG 400 and PEG 4000 and three-stage with PEG 400, PEG 1500 and PEG 4000. The data received from analyses of both volume and surface gave detailed information about the success of each conservation method. Attempts were made to quantify the damage patterns, specifically shrinkage, collapse, and cracks. While PEG and freeze-drying, alcohol-ether-resin, as well as the Kauramin 800® method gave the best results, analysis also highlighted the failures of each method.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call