Abstract
In the present study FTIR, SEM and EDAX analysis are carried out for better understanding of morphology of samples with two different silicone rubber formulations subjected to inclined plane tracking test for both with and without UV radiations of different intensities. The morphological behavior of the material is also given for polluted samples after they have undergone inclined plane tracking test with UV super imposed. The surface composition of Silicone rubber from EDAX analysis indicated no significant change in elemental levels of Silicone(Si), carbon(C) and oxygen(O) prior to UV exposure. However the reduction in the element Aluminium(Al), is significant in specimens subjected to test as per IEC 60587, in the presence of UV radiations and also for samples after 1000 hours UV exposure. It is also inferred from the study that, the intensity of UV radiation during inclined plane tracking test and long duration UV exposure in weather o meter plays a major role in deteriorating the surface characteristics of the material.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have