Abstract

ABSTRACTA method for the determination of lead is described using thiol-functionalized gold nanoparticle. The detection method is based on the prevention of thiol-induced aggregation of gold nanoparticles by lead. Among six thiols, e.g., 4-mercapto-1-butanol, meso-2, 3-dimercaptosuccinic acid, mercaptosuccinic acid, 6-mercapto-1-hexanol, 4-(methylthio)-1-butanol, 1-propanethiol, four (4-mercapto-1-butanol, 6-mercapto-1-hexanol, 4-(methylthio)-1-butanol and 1-propanethiol) induced the aggregation of the gold nanoparticles which was measured by the change in absorbance at 520 and 650 nm. Prior incubation of the gold nanoparticles with lead decreased the 4-(methylthio)-1-butanol-induced aggregation of gold nanoparticles in a dose-dependent manner. A linear inverse relationship between the logarithmic concentration of lead and the ratio of absorbance at 650 to 520 was noted. The method has a dynamic range from 10 nM to 100 µM. However, metals such as mercury and chromium were more effective in comparison with lead in preventing the 4-methylthio-1-butanol-induced aggregation of gold nanoparticles. The method can be used for assessing the heavy metal load in water samples.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.