A simple solution combustion synthesis route for preparation of Cu-doped SrAl 4O 7 has been described. Average particle size of 33 nm and platelet-like morphology has been observed. ESR studies confirm the presence of Cu in polycrystalline SrAl 4O 7. Bright-green luminescence under near-UV irradiation arising due to transition between Cu + levels with microsecond level decay time makes it suitable for application in phosphor converted light emitting diode (LED). TL measurements show broad glow peaks which when deconvoluted indicate activation energies in the range of 0.6–1.1 eV and elucidate the trapping dynamics.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.