Abstract

The prescribed initial density of the material before loading was achieved by different methods: free pouring of powder, prior Static pressing, and prior explosive pressing. The original material density, loading conditions, and density of the compacts obtained are indicated in Table i. In experiment 4 after free pouring of the aluminum nitride powder it was preliminarily compressed by an explosion by loading scheme I with a peak pressure amplitude of 2 GPa.