Transparent luminescent Y0.98−xBixEu0.02VO4 (0<x<1) ceramic films have been prepared using a polymeric route and heat-treatment at 550°C. A solid solution of zircon-type Y1−xBixVO4 is obtained for x values below 0.5 whereas phase separation is observed above this limit. The absorption spectra of the films show a shift of the band edge towards high wavelength with the bismuth content, as theoretical calculi have predicted. Luminescence of the films under a UV excitation is typical of europium ion in the zircon structure. The poor correlation between absorption and excitation spectra at high bismuth content is coherent with desexcitation in localized states of valence band. However, the excitation wavelength could still be tuned from deep-UV to near-UV range by inserting bismuth in YVO4.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.