Abstract

Alloys with composition of AlCoCrFeNiTix (x: molar ratio; x=0,0.5,1,1.5) were designed by using the strategy of equiatomic ratio and high entropy of mixing. The alloy system is composed mainly of body centered cubic solid solution and possesses excellent room-temperature compressive mechanical properties. Particularly for AlCoCrFeNiTi0.5 alloy, the yield stress, fracture strength, and plastic strain are as high as 2.26GPa, 3.14GPa, and 23.3%, respectively, which are superior to most of the high-strength alloys such as bulk metallic glasses.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.