ABSTRACTThe preparation of μc-Si films from SiH4-H2 mixtures by electron-cyclotron resonance (ECR) CVD at deposition temperatures ≤ 400°C on foreign substrates is reported. Deposition conditions were identified for which Si films with a high degree of crystallinity were grown as was confirmed by Raman spectroscopy. A factorial analysis was carried out, for which the influence of deposition temperature, microwave power, hydrogen dilution and total pressure on film growth were investigated. Samples of optimized crystallinity were prepared in a lowpressure and high-hydrogen dilution regime. In-plane grain sizes were measured by TEM and found to be on the order of 10 - 12 nm. Next to the optimization of crystallinity several sources of impurity contamination during film deposition were identified and eliminated. Intrinsic μc-Si layers could be prepared under these conditions that exhibited a dark conductivity σd of 2 × 10-7 S/cm and photosensitivity σph/σd of 150. It is concluded that ECR CVD is capable of producing intrinsic layers with electronic properties as necessary for use in state-of-the-art n-i-p μc-Si solar cells.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.