Abstract

The effects of Ni on the properties of the Sn-2.5Ag-0.7Cu-0.1Re solder alloy and its creep properties of solder joints are researched. The results show that with adding 0.05wt% Ni in the Sn-2.5Ag-0.7Cu-0.1Re solder alloy, the elongation can be sharply improved without decreasing its tensile strength and it is 1.4 times higher than that of the commercial Sn-3.8Ag-0.7Cu solder alloy. Accordingly the creep rupture life of Sn-2.5Ag-0.7Cu-0.1Re-0.05Ni solder joints is the longest, which is 13.3 times longer than that of Sn-2.5Ag-0.7Cu-0.1Re and is also longer than that of the commercial Sn-3.8Ag-0.7Cu solder alloy. In the same environmental conditions, the creep rupture life of Sn-2.5Ag-0.7Cu-0.1Re-0.05Ni solder joints can sharply decrease with increasing the temperature and stress.