Abstract
This paper investigates application of slow strain rate tensile (SSRT) testing as a laboratory method to characterize stress corrosion cracking (SCC) susceptibility of type 40Cr steel in the acidic chloride solution. SSRT testing was carried out at room temperature in acidic chloride solution and seawater at different strain rates (3.82×10-7 to 1.41×10-6 s-1),respectively. The results show that the type 40Cr steel is susceptible to stress corrosion cracking in a certain strain rates (around 1.41×10-6 s-1) in the acidic chloride solution. In tests performed at this strain rate (1.41×10-6 s-1), while the specimens are not susceptible to SCC in seawater. Typical intergranular attack is seen on the fracture surface of the former that had failed due to SCC, and the latter had underwent considerable necking before fracture, also represented by high reduction of area (RoA) and fractographic feature of dimples consistent with ductile failure. Additionally, the results are consistent with the data of electrochemical noise (EN) that is generated of type 40Cr steel exposed to the acidic chloride solution and seawater. This study also supports SSRT and EN technique as an effective testing technique for SCC studies.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.