A novel microstructure evolution mechanism is proposed to optimize the preparation process of superalloy powders. This study focuses on the solidification segregation, as well as the correspondence between the powder sizes and the microstructure evolution mechanism of Ni-based superalloy fine powders. The quantitative analysis was systematically examined using thermodynamic analysis. The results indicated that dendrites and cellular microstructures formed on the surface and interior of the powders, but their key distribution characteristics were highly related to both the powder size and ultra-fine satellite particles that adhered to its surface. The number of ultra-fine satellite particles, outgrowth index, spacing between the secondary dendrite arms increased with the increasing powder size, exhibiting an ideal linear relationship. In particular, when the powder size was small, the length of the internal primary dendrite arms increased as the powder particle size increased, but interestingly, remained at approximately 30 μm when the particle size exceeded 45 μm. Finally, a model for the microstructural evolution mechanism of the surface and interior of alloy powders ≤100 μm was developed, which lays the theoretical foundation for the preparation of superalloy powders.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.