In high speed machining superalloys processes, tool wear is strongly influenced by the cutting temperature and contact stresses. Finite element analysis of machining can be used as a supplementary to the physical experiment, this paper provides investigations in 2D and 3D finite element modeling and simulation of prestressed cutting for GH4169 superalloy, a tool wear model for the specified tool and workpiece pair is developed based on the Usui's wear model, furthermore, tool temperature, wear rate and nodal displacement on the face of tool in prestressed cutting of superalloy is analyzed under various prestress condition and cutting parameters, and Python language is adopted to modify the Abaqus code used to allow tool wear calculation and tool geometry updating. The results of the simulation indicate that the tool wear rate increases with the increase of cutting time, and the influence of the prestress to tool wear in prestressed cutting process of shaft part is unremarkable.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have