Abstract

Membrane silica scaling hinders sustainable water production. Understanding silica scaling mechanisms provides options for better membrane process management. In this study, we elucidated silica scaling mechanisms on an asymmetric cellulose triacetate (CTA) membrane and polyamide thin-film composite (TFC) membrane. Scaling filtration showed that TFC membrane was subjected to more severe water flux decline in comparison with the CTA membrane, together with different scaling layer morphology. To elucidate the silica scaling mechanisms, silica species in the aqueous solution were characterised by mass spectrometry as well as light scattering. Key thermodynamic parameters of silica surface nucleation on the CTA and TFC membranes were estimated to compare the surface nucleation energy barrier. In addition, high resolution X-ray photoelectron spectroscopy resolved the chemical origin of the silica-membrane interaction via identifying the specific silicon bonds. These results strongly support that silica scaling in the CTA membrane was driven by the aggregation of mono-silicic acid into large silica aggregates, followed by the deposition from bulk solution onto the membrane surface; by contrast, silica polymerised on the TFC membrane surface where mono-silicic acid interacted with TFC membrane surface, which was followed by silica surface polymerisation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.