Abstract

The physical integrity and photocatalytic performance of titanium dioxide (TiO2) deteriorate with aging. Here we propose a pre-treatment with nitric or sulfuric acid of commercial TiO2 nanopowders used in coating, mortars, or paints. The diffuse reflectance is increased between 1500 and 2500 nm by 0.04 and 0.06, respectively, with nitric and sulfuric acid (unaffected by neutralization). Nitric acid causes a decrease in crystallinity and photocatalytic activity, which drops by almost 20%; this drawback is prevented by post-treatment neutralization, which allows to recover initial photocatalytic efficiency and even increase it. Treatment with sulfuric acid shows no significant effect on photoactivity, instead.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.