High pressure acid leaching (HPAL) is the primary method for extraction of nickel from limonitic laterite. The severe operating conditions, the complexity of facilities, and several technical problems, such as scale formation, have always accompanied the HPAL, however. In this paper, the selective acid leaching of nickel from the pre-reduced limonitic laterite under moderate HPAL conditions was studied. For the calcine with reduction degree of 93.4%, about 88.2% nickel could be selectively extracted at 100?C with an acid/ore ratio of 0.164, leaving less then 5.0g/L iron in the solution. Further increase of leaching temperature, and the ensuing dehydration, transformed goethite in the leaching residue to hematite. When the temperatures were as high as 180?C, the recovery of nickel increased to 95.2%, within one hour, depressing the residual soluble iron to below 1.0g/L (pO2= 1.0 MPa, acid/ore= 0.287).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.