Abstract

Abstract 1012 and S12C are wrought low-carbon (carbon = 0.10–0.15 percent) non-alloy steels that are used in the as rolled, annealed, normalized, or cold worked condition. These steels are characterized by low strength, high ductility, excellent cold formability, and excellent weldability. Within the carbon range of these steel grades, strength and hardness will increase with increase in carbon content and with cold work. Such increases in strength are at the sacrifice of ductility or the ability to withstand cold deformation. Grades 1012 and S12C are widely used for lightly stressed parts that require higher strength levels than can be achieved by the lower carbon grades and for applications where cold formability is the primary requisite. They are less expensive than 1008 and can be used when the requirements for cold forming are less exacting. 1012 and S12C may also be used in the case hardened, nitrided, or nitrocarburized condition. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on low and high temperature performance as well as forming and heat treating. Filing Code: CS-268. Producer or source: Heat Treater's Guide.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.