Abstract
Lightweight magnesia aggregates were fabricated using high-purity MgO agglomerates with the addition of Mg(OH)2 as a pore former. The pore evolution and its relationship to the resulting properties were investigated. Mg(OH)2 decomposition increased the number of inter-agglomerate pores, which subsequently affected the porosity and pore structure. When Mg(OH)2 was 0–20 wt%, the inter-agglomerate pores were converted to both open and closed small pores, which effectively reduced the thermal conductivity and improved the thermal shock resistance (TSR) by accommodating thermal stress and inducing crack deflection. Small pores also favored the formation of a dense (Mg, Fe)O corrosion layer, preventing further slag penetration. However, large open pores occurred with further increasing Mg(OH)2 content, which dramatically deteriorated the TSR and slag resistance. The specimen with 20 wt% Mg(OH)2 exhibited the best overall performance, with a thermal conductivity of 16.6 W/(m·K) at 500 °C, and a residual flexural strength ratio of 32.3%; its slag resistance was comparable with that of dense magnesia.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.