Abstract
In the previous period of work, twelve overlay hardfacing alloys were selected for erosion testing based upon a literature review. All twelve coatings were deposited on 1018 steel substrates using the plasma arc welding process. Ten samples from each coating were prepared for erosion testing. The coating deposition and sample preparation procedures were described in the previous quarterly report. During the past quarter, all the coatings were erosion tested at 400 C. The erosion resistance of each coating was evaluated by determining the steady state erosion rate. In addition, the microstructure of each coating was characterized before and after the erosion tests. This progress report describes the erosion test results and coating microstructures. Also, a preliminary analysis on the relationships, between weld overlay coating hardness, microstructure, and erosion resistance will be discussed.