Abstract

The results of the conducted experimental studies aimed at conducting X-ray studies of tungsten-titanium-cobalt hard alloy made by spark plasma sintering of carbide powders obtained by electroerosive dispersion of T5K10 hard alloy waste in kerosene are presented. It is shown that the obtained new hard alloys have a fine-grained structure, elemental and phase compositions identical to the original dispersible hard alloy of the T5K10 grade.